PMID- 1593429 OWN - NLM STAT- MEDLINE DCOM- 19920702 LR - 20190819 IS - 0886-3350 (Print) IS - 0886-3350 (Linking) VI - 18 IP - 3 DP - 1992 May TI - Fibrinous reaction on implanted intraocular lenses. A comparison of conventional PMMA and heparin surface modified lenses. PG - 236-9 AB - We studied the fibrinous reaction after intraocular lens (IOL) implantation in the posterior chamber of cynomolgus monkeys. In 50% of the eyes, we implanted an IOL made of conventional poly-(methyl methacrylate) (PMMA); in the remaining eyes we implanted a PMMA IOL with a heparin modified surface. Two, 4, 8, and 18 weeks after surgery the eyes were examined by slitlamp for fibrinous reactions on and around the IOL surface. At weeks 4, 8, and 18 there was a marked decrease in fibrinous reaction in the eyes with a heparin surface modified IOL. The results of this study accord with earlier findings that heparin surface modification improves the biocompatibility of the IOL. FAU - Lundgren, B AU - Lundgren B AD - Kabi Pharmacia Ophthalmics, Department of Biology, Uppsala, Sweden. FAU - Selen, G AU - Selen G FAU - Spangberg, M AU - Spangberg M FAU - Harfstrand, A AU - Harfstrand A LA - eng PT - Comparative Study PT - Journal Article PL - United States TA - J Cataract Refract Surg JT - Journal of cataract and refractive surgery JID - 8604171 RN - 0 (Methylmethacrylates) RN - 9001-31-4 (Fibrin) RN - 9005-49-6 (Heparin) SB - IM MH - Animals MH - Cataract Extraction MH - Female MH - Fibrin/*biosynthesis MH - Foreign-Body Reaction/metabolism MH - *Heparin MH - *Lenses, Intraocular MH - Macaca fascicularis MH - Male MH - *Methylmethacrylates MH - Surface Properties EDAT- 1992/05/01 00:00 MHDA- 1992/05/01 00:01 CRDT- 1992/05/01 00:00 PHST- 1992/05/01 00:00 [pubmed] PHST- 1992/05/01 00:01 [medline] PHST- 1992/05/01 00:00 [entrez] AID - S0886-3350(13)80899-1 [pii] AID - 10.1016/s0886-3350(13)80899-1 [doi] PST - ppublish SO - J Cataract Refract Surg. 1992 May;18(3):236-9. doi: 10.1016/s0886-3350(13)80899-1.